British Petroleum (BP) Offshore Blind Pipe Test Probability of Detection (POD)
This test was designed to determine the probability of detection (POD) for contact point corrosion on an offshore pipe furnished by British Petroleum (BP). The piping specifications are three and a half (3.5) outside diameter (OD) x three hundred thousandths (0.300”) schedule (SCH) eighty (80), spanning seventy (70) inches in length, and made of carbon steel. The test was initially performed as a blind test, with the damaged area hidden under a wax wrap. Permission was obtained to create multiple inspection points through the wrap, approximately the size of a dime, to conduct our testing over the concealed area. Ultrasonic testing (UT) thickness measurements were also taken as an additional inspection method.
The inspection results revealed a low level of outside diameter (OD) corrosion, with wall loss ranging from eleven (11) percent to twenty (20) percent throughout the pipe. However, the area spanning forty (40) inches to fifty (50) inches exhibited a significantly higher test average compared to the calibration baseline average. Based on our calibration curves, the indication showed a fifty-six (56) percent wall loss, with a remaining wall thickness of one-hundred and forty thousandths (0.140”). Following the initial test, we removed the wrapped covering over the damaged area to initiate discovery work and conduct manual ultrasonic thickness (UT) readings.
Following the removal of iron oxide flakes from the outside diameter (OD), our examination revealed lake-type corrosion and pitting. This sample exhibited corrosion ranging from large volume shallow defects to small deep corrosion. We successfully located the deepest corrosion pit and conducted ultrasonic (UT) measurements in the forty (40) inches to fifty (50) inches area, which indicated a remaining wall of one-hundred and forty-seven thousandths (0.147”) equivalent to fifty-four percent (54%) wall loss. Upon reviewing the damaged areas, we observed both large volume shallow corrosion and small volume deep corrosion defects, which VIR accurately detected. This test was performed at seventy (70) inches. Please refer to Figure 9.

Figure 9 . VIR Report illustrates Wrapped Pipe and Results

Brian K. Beresford “Bear”
Sole Proprietor
(832) 943-0979
10 Rosalie Street
Shepherd, Texas 77371