Corrosion Under Insulation (CUI)

A twenty-four (24) inch flare header with a wall thickness of 0.375 inches, fabricated from SA-53 Grade B carbon steel insulated piping, underwent VIR inspection. Ultrasonic testing (UT) inspection ports were installed at five (5) foot intervals at twelve (12) o’clock, three (3) o’clock, six (6) o’clock, and nine (9) o’clock positions. VIR sensors were inserted through the UT ports to obtain VIR readings. A scan conducted at position A-B at the six (6) o’clock position revealed a fifty-five (55) percent wall loss, with a remaining wall thickness of 0.167 inches. Furthermore, automated ultrasonics testing (AUT) revealed a fifty-three (53) percent wall loss. Wall loss was also observed at the support structures during the inspection. Please refer to Figure 5.

Corrosion Under Insulation

Figure 5 . Drawing with VIR results and Automated Ultrasonic Testing (AUT) Validation

VIR Systems logo tm

Brian K. Beresford “Bear”

Sole Proprietor
(832) 943-0979

10 Rosalie Street
Shepherd, Texas 77371