Hydrogen Induced Cracking and Blistering (HICB)
Results from Laboratory Testing
Laboratory results are vital to perform in order to determine diverse applications for the technology and sensitivity levels. The testing of burred pipe underground and VIR fully submerged underwater worked effectively with no interference. Material sorting, flange face corrosion, and pipe temperature assessments were conducted with positive results. The twelve thousand (1,200) pound steam pipe test indicated that the technology effectively identified the smallest ligament of damage without averaging the wall loss. The most significant surprise was the detection of Hydrogen Induced Cracking (HIC) in its initial stages, where it is undetectable to ultrasonics. Here are some of the surprising findings.
- VIR works when its fully submerged under water
- VIR was performed underground successfully
- Material sorting with positive results
- Flange face corrosion study was performed with positive results and needs more development
- Pipe Temperature study was performed
- Exchanger study was performed with positive results and needs more development
- Offshore Scab Samples Proven Technology
- Twelve Thousand (1,200) Pound Steam Pipe
- Hydrogen Induced Cracking (HIC) attach lab results.
Twelve Thousand (1,200) Pound Downstream Steam Pipe
San Jacinto College provided a twelve thousand (1,200) pound steam pipe sample for testing using VIR technology. The pipe’s dimensions were three and a half (3.5) inches in outside diameter (O.D.), half inch (1/2”) wall thickness, and twelve (12) inches in length. The sample piece, situated downstream from a partially opened valve, had been removed from service. This test aimed to investigate the effects of large, tapered erosion on the inside diameter (ID) of a pipe and assess the sensitivity of VIR technology on a partial pipe. The results showed that VIR technology effectively identified the smallest ligament of damage without averaging the wall loss. The sample pipe was cut in half for a visual examination of the damage.
San Jacinto College submitted three (3) samples, verified through metallurgical analysis, with dimensions of eleven (11) inches by four (4) inches by one (1) inch. The plates were tested every two (2) inches along their lengths. The first plate was free of defects, the second in its initial stages of early Hydrogen Induced Cracking (HIC) where it is undetectable to ultrasonics, and the third displayed visible hydrogen-induced cracking and blistering. The VIR readings were zero for the undamaged plate, 5.3 for the plate with nascent Hydrogen Induced Cracking (HIC), and 10.6 for the plate with visible HIC and blistering. VIR is sensitive to changes even within the grain boundaries of the material. Please refer to Figure 10.

Figure 10 . VIR Report Hydrogen Induced Cracking (HIC)

Brian K. Beresford “Bear”
Sole Proprietor
(832) 943-0979
10 Rosalie Street
Shepherd, Texas 77371